Precipitation on can bottom of inert components, high specific weight pigments or particles which cannot be kept dispersed into paint
| REASON | SOLUTION |
| Storage time has been too long. | It is necessary to stir the paint, as stronger as thicker and more consistent settling is. in some cases, it could be necessary a mechanical and long-lasting stirring. In extreme cases, it could be necessary to substitute the product. |
| An excess of dilution provokes the lowering of viscosity, accelerating the sedimentation of bigger particles. | |
| Lack of wetting agents due to wrong formulation of paint. |